Lasmetaal biedt optimale sterkte en oxidatieweerstand boven 815 °C (1500 °F) tot 1149 °C (2100 °F), vooral bij het lassen op basismetalen van nikkel-ijzer-chroomlegeringen.
E Ni 6617(NiCr22Co12Mo), ENiCrCoMo-1, 2.4628
2.4663, 2.4851, 1.4876, 1.4859, 1.4952, 1.4958, 1.4959,
NiCr21Co12Mo, NiCr23Co12Mo, NiCr23Fe, X6CrNiNbN 25 20, X5NiCrAlTi 31 20, X8NiCrAlTi 32 21, X10 NiCrAlTi 32 21, GX10 NiCrSiNb 32 20,
UNS: N06601, N06617, N08810, N08811
Inconel Alloys 600 and 601, Incoloy Alloys 800 HT and 802 and cast Alloys such as HK-40, HP and HP-45 Modified, Alloy 617,
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Impact Energy (J) ISO-V | Hardness |
---|---|---|---|---|---|
RT | |||||
As Welded | 480 | 760 | 32 | 120 | HRc |