Very good abrasion resistance in combination with impact even at higher temperatures up to 550ºC. To much layers should be avoided, preheat is necessary to avoid cracking. A buffer layer with OA 4370 or OA MnCr is recommended in case of sensible base material or old layers. Weldable without protective gas.
Cement pumps, Crusher bars, Hammer and Blooming table rolls, Mineral and Brick industry.
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Hardness |
---|---|---|---|---|
As Welded | 60 HRc |