ER 383 is used to weld base metals of similar composition to itself or to other grades of stainless steel. ER383 contains a low maximum of carbon, silicon, and sulfur to decrease the hot cracking and fissuring, while maintaining the resistance to corrosion.
Alloy 825 N08825 , Alloy 825 h Mo N08821, Alloy 28 and Alloy 20 ( X1NiCrMoCu31-27-4 ), Alloy 904L ( X1NiCrMoCu25-20-5 ), 1.4563, 1.4539, NiCr 21 Mo 2.4858, NiCr 21 Mo 6Cu 2.6410, X3NiCrCuMoTi27-23 1.4503
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Impact Energy (J) ISO-V | Hardness |
---|---|---|---|---|---|
RT | |||||
As Welded | 380 | 570 | 38 | 100 | HRc |