The weld deposit offers good wear and corrosion resistance even in seawater. Welding instructions: - Preheating for sections >6 mm from 150 till 300 ºC is recommended. Use the normal standard welding techniques.
Aluminium bronze, Cladding steel, Shafts, Gliding surfaces, Joining steel to, Aluminium Bronze or Copper, etc.
Mat.n: 2.0916, 2.0920, 2.0928, 2.0460, 2.0932
CuAl5, CuAl8, G-CuAl9, CuZn20Al2, CuAl8Fe3,
UNS: C60600, C61000, C68700, C61400, Copper-beryllium alloys Cu+0.5-2%Be, Cu-Zn brasses, Aluminum brass Cu22%, Zn2%Al, Manganese bronzes Cu+20-45%Zn+1-3%Mn, Silicon bronzes Cu+1-3.5%Si
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Hardness |
---|---|---|---|---|
As Welded | 200 | 450 | 24 | 150 HB |