Cromarod 309 MoL
CEWELD® 4829 MoTi is for joining heat resistant CrNi-steels of the same kind and also joining dissimilar alloys such as steel to stainless steel. Cladding on low alloyed steels in case a 18/8/2 CrNiMo layer is required in the first layer.
CEWELD® 4829 MoTi is for joining heat resistant CrNi-steels of the same kind and also joining dissimilar alloys such as steel to stainless steel. Cladding on low alloyed steels in case a 18/8/2 CrNiMo layer is required in the first layer.
The increased ferrite content (FN~19) in the weld metal of CEWELD® 4829 MoTi enables high crack resistance with materials that are less suitable for welding. Particularly easy processing with very good seam appearance, both with direct and alternating current. Self-lifting slag. For application temperatures from -60ºC to 300ºC, for 1st layer weld claddings up to 400ºC.
23% Cr, 12%Ni, 3% Mo, 309LMo
1.4401, 1.4404, 1.4406, 1.4410, 1.4437, 1.4571, 1.4580, 1.4459, 1.4513, 1.4521, 1.4526, 1.4113, 1.4575
AISI 436, 444, 434
UNS S43600, S 44400, S43400,
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Impact Energy (J) ISO-V | Hardness |
---|---|---|---|---|---|
RT | |||||
As Welded | 460 | 650 | 32 | 55 | HRc |