Böhler Q G 307
CEWELD 307Si is for buffer layers before hardfacing, dissimilar welding between steel and stainless steel, armor plate, exhaust systems (type 409, 304), high Manganese austenitic steel, heterogeneous welding, difficult to weld steels etc. The deposit work hardens from 200 HV to 450 HV.
CEWELD 307Si is for buffer layers before hardfacing, dissimilar welding between steel and stainless steel, armor plate, exhaust systems (type 409, 304), high Manganese austenitic steel, heterogeneous welding, difficult to weld steels etc. The deposit work hardens from 200 HV to 450 HV.
Corrosion resistance is equivalent to type 304, high mechanical properties and good weldability, work hardening and cold-tough to -196°C.
19% Cr / 9% Ni / 7% Mn, ISO 15608: 8.1 Cr ≤ 19 %
1.3401, 1.5637, 1.5680, 1.4370
X 20 Cr 13, X 8 Cr 17, X 22 CrNi 17, X 5 CrNi 17, G-X 20 Cr 14 mix S355
42CrMo4, C45, 42MnV7, X120Mn12, 10 Ni 14, 12 Ni 19 etc.
ASTM 307, 304, (409, 403, 405, 410, 420, 430, 440, 501, 502)
Amor
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Impact Energy (J) ISO-V | Hardness |
---|---|---|---|---|---|
-196°C | |||||
As Welded | 400 | 600 | 40 | 40 | HRc |