BASINOX 410 S

Brand
Ceweld product
Type
Basic coated rod electrode with approx. 13% Cr. (type E410, 1.4009)
classification
AWS
A 5.4: E 410-26
EN ISO
3581-A: E 13 B 42
W.Nr.
1.4009
Applications

CEWELD®  4009 Ti can be used for welding martensitic-ferritic steels and cast steel. Predominantly for build-ups, corrosion-resistant and wear-resistant layers. Preferred applications are sealing surfaces on gas, water and steam fittings at operating temperatures of up to 450ºC.

Type
Basic coated rod electrode with approx. 13% Cr. (type E410, 1.4009)
Applications

CEWELD®  4009 Ti can be used for welding martensitic-ferritic steels and cast steel. Predominantly for build-ups, corrosion-resistant and wear-resistant layers. Preferred applications are sealing surfaces on gas, water and steam fittings at operating temperatures of up to 450ºC.

Properties

CEWELD® E 4009 Ti can be used for a working temperature of up to 450ºC. The recommended preheat temperature is 200ºC - 300°C unless the base material requires a higher preheat temperature. Use DC+ polarity and min 2 layers are required. A tempering of 700 - 750°C is possible if required.

Classification
AWS
A 5.4: E 410-26
EN ISO
3581-A: E 13 B 42
F-nr
1
FM
5
W.Nr.
1.4009
Suitable for

Ferritic 13 % Chrome steel,

1.4000, 1.4001, 1.4002, 1.4003, 1.4006, 1.4008,  1.4021, 1.4024, 

X6Cr13, X6CrAl13,  X10Cr13, X15Cr13, X20Cr13, G-X10Cr13

AISI 410, 420

Approvals
CE
Welding positions
PA
PB
PC
PF
Redrying
300°C / 2 hr
Analysis
C Si Mn P S Cr Ni Mo Nb N Cu Ta Nb+Ta W
0.1 0.6 0.7 13 0.2 0.5
Mechanical Properties
Heat
Treatment
RP0,2
(MPa)
Rm
(MPa)
A5
(%)
Hardness
725°C- 755°C 1h 500 650 21 180 HB
As Welded 550 800 10 300 HV