- Produktspezifikationen
- Verpackung
- Bitte um Angebot
Machinable ,Heat resistant weld deposit with excelent wear resistance. The weld deposit can be heat treated to offer maximum service protection.
45-52 HRc
1.2567, 1.2365, 1.2713, 1.2714, 1.2581
30WCrV17 2, 32CrMoV12-283, 55NiCrMoV6, 55NiCrMoV7, X30WCrV9-3
Tempering : approx. 3 h / temperature depending on desired working hardness.
Soft annealing : 2 - 4 h at 800° C -840° C / furnace cooling
Heat Treatment |
RP0,2 (MPa) |
Rm (MPa) |
A5 (%) |
Hardness |
---|---|---|---|---|
As Welded | 47 HRc | |||
580°C±15°C 1h | 53 HRc |